Spectrographic Analysis Of Sand Quartz And Quartz Glasses And The Method Of Standard Preparation (In Polish)

The advantages of spectrographic method in the glass institute have been described. The preparation methods and testing of standards are given. The precision and accuracy of determinations are presented.