Spectral Transmittance Of Christiansen Filters - Experimental Observations

The spectral transmittance of an inhomogeneous medium consisting of a powder of a transparent solid material immersed in a different material, such as a liquid, depends on the difference of refractive indices of both materials. If these coincide, the spectral transmittance is maximum. With increasing absolute difference of the refractive indices, the spectral transmittance of a direct beam of electromagnetic radiation decreases. This is the origin of a bell-shaped transmittance curve of the inhomogeneous medium. A plane-parallel layer of such a medium is called the Christiansen filter, in honour of the author who described this effect more than 100 years ago.

Author
H J Hoffmann & R Steinhart
Origin
Technische Universitat Berlin, Germany
Journal Title
Glastech Ber Glass Sci Technol 71 11 1998 319-326
Sector
Special Glass
Class
S 1605b

Request article (free for British Glass members)

Spectral Transmittance Of Christiansen Filters - Experimental Observations
Glastech Ber Glass Sci Technol 71 11 1998 319-326
S 1605b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.