Spectral Properties Of Bi-Er-Yb Triply-Doped Borosilicate Glasses With 805Nm Excitation

Spectral properties of Bi-Er-Yb triply doped borosilicate glasses with different concentrations of bismuth were investigated. Broad absorption bands appeared at 300-1700nm and the emission bands in near infrared and visible wavelength regions from E43+ and Yb3+ ions showed efficient enhancement in peak intensity due to the incorporation of bismuth upon excitation at 805nm. Possible energy transfer mechanisms of E43+, Yb3+ and bismuth ions were proposed.

Author
D H Son Et Al
Origin
Gwangju Institute Of Science, S Korea
Journal Title
Ceramic Transactions Vol 231 2012 209-217 (Proc 9Th Int Conf On Advances In Fusion (Afpg9), Australia
Sector
Glass Fibre
Class
GF 746

Request article (free for British Glass members)

Spectral Properties Of Bi-Er-Yb Triply-Doped Borosilicate Glasses With 805Nm Excitation
Ceramic Transactions Vol 231 2012 209-217 (Proc 9Th Int Conf On Advances In Fusion (Afpg9), Australia
GF 746
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.