Spacer Alternatives For Saving Energy

Spacer technology has become important for the insulating glass industry because it allows IG manufacturers to differentiate their products from the competition. The introduction of new spacers has brought awareness of the various factors which affect the working life span of sealed units, such as moisture vapour transmission, argon gas retention and UV degradation.