It has been announced that offers have been made by French, Swiss and Saudi investors to buy a 51% stake of the capital of Tunisian glass bottle manufacturer Societe Tunisienne de Verreries (SOTUVER). The offers were in response to an international tender launched last April by Tunisia as part of its privatisation programme.