Some Thoughts On The Strength Of Lightweight Glass Containers

The requirements for producing strong lightweight containers are discussed with particular reference to carbon-based handling materials and chemical processes for surface treatment.

Author
H P Williams
Origin
Hermann Heye
Journal Title
Glastech Ber 1989 62 3 83-87
Sector
Container glass
Class
C 200

Request article (free for British Glass members)

Some Thoughts On The Strength Of Lightweight Glass Containers
Glastech Ber 1989 62 3 83-87
C 200