Some Recent Advances In Glasses And Glass-Ceramics

Novel compositions and applications are discussed. These include durable low temperature glasses, durable far-infrared transmitting glasses, full-colour photosensitive glasses, glass microlens arrays, precision direct moulding, specialised glass-ceramics for dental restorations, for film or paper, or for tough materials.

Author
G P Smith
Origin
Corning Glass Works
Journal Title
Materials And Design 1989 X 2 March/April
Sector
General
Class
G 490