Solving Firing Problems - Guessing Or Facts

In this paper the author discusses a process of elimination, often necessary to first determine where the problem is occurring before attempting to come up with a solution. Travelling thermocouples and the black coring zone are also covered.

Author
J Brown
Origin
General Shale Products, Usa
Journal Title
Am Ceram Soc Bull 75 2 1996 67-68