Solar Glasses: A Case Study On Semitransparent Organic Solar Cells For Self-Powered Smart, Wearable Devices

This paper reports on solution-processed, semitransparent organic solar cells that are implemented as lenses in sunglasses. The electrical power provided by the lens-fitted solar cells sustains a microelectronic circuit that is used to read out temperature and illumination intensity sensors and to make this information available on two displays integrated into the temples of the Solar Glasses. The microelectronic circuit is designed to operate at illumination intensities down to 500 lux, rendering the Solar Glasses suitable for outdoor and indoor use as well as for operation in diffuse light. Hence, this case study provides an example for consumer-oriented mobile applications, self-powered by integrated solar cells, which specifically exploit the unique properties of organic solar cells. The article is free to download in full from the above-mentioned link.

Author
D Landerer Et Al
Origin
Energy Technology June 2017
Journal Title
Open Access: Onlinelibrary.Wiley.com/Doi/10.1002/Ente.201700226/Full
Sector
Special Glass
Class
S 4387

Request article (free for British Glass members)

Solar Glasses: A Case Study On Semitransparent Organic Solar Cells For Self-Powered Smart, Wearable Devices
Open Access: Onlinelibrary.Wiley.com/Doi/10.1002/Ente.201700226/Full
S 4387
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.