Sol-Gel Optical Coatings For Lasers, Iii

Highly reflective and polarising sol-gel-derived optical coatings have been prepared and tested for the proposed French megajoule neodymium-glass laser.

Author
H G Floch Et Al
Origin
Centre D'Etudes De Limeil-Valenton Villeneuve St George'S, France
Journal Title
Am Ceram Soc Bull 74 12 1995 48-52
Sector
Special Glass
Class