Sol-Gel Optical Coatings For Lasers, Ii

Antireflective sol-gel-derived optical coatings have been prepared and tested for the proposed French megajoule neodymium-glass laser.

Author
H G Floch Et Al
Origin
Cea, France
Journal Title
Am Ceram Soc Bull 74 11 1995 84-89