Small Angle X-Ray Scattering And Electron Paramagnetic Resonance Studies Of Nucleation And Crystallisation In Basalt Glasses

Small angle X-ray scattering, wide angle X-ray diffraction and electron paramagnetic resonance measurements on tholeitic basalt glasses prepared under various redox conditions are reported.