Small Angle Neutron Scattering Study Of Phase Separation In The Binary Glass System Tio2-Sio2

Absence of separation in a glass with 9.5% TiO2 heated to 1200 degrees C was confirmed and phase separation was observed when the TiO2 content was increased to 14.7%.