Slecting The Highest Annealing Temperature For Glass Strip

Laboratory experiments have been carried out in which glass laths were annealed after preliminary cooling to different transition temperature values under natural convection conditions.

Author
Nv Lalykin And As Makhnavetskii
Origin
Unknown
Journal Title
Glass And Ceramics 38 5-6 1982 226-228