Size Scaling Of Tensile Failure Stress In A Float Soda-Lime-Silicate Glass

The (tensile) strength-size scaling of a float-soda-lime-silicate glass was studied using biaxial flexure & Hertzian ring crack initiation testing. The examined Weibull effective areas spanned ~0.4-48,000mm2. Both the air & tin sides were tested. The air side was stronger than the tin side as others have observed; however, the differences in their characteristic strengths decreased with a decreasing effective area & their strengths converged for effective areas smaller than ~100mm2. The failure stress at the smallest effective area examined for the tin side was ~500% greater than that at the largest effective area, while that difference was ~250% for the air side. A Weibull modulus change at ~100mm2 suggests different strength-limiting flaw types were dominant below & above this effective area. Results reinforce the importance of the interpretation & use of the tensile strength of glass in context to how much of its area is being subjected to tensile stress.

Author
A A Wereszczak Et Al
Origin
Oak Ridge Nat Labs, Usa
Journal Title
Int J Appl Glass Sci 1 2 2010 143-150
Sector
Flat glass
Class
F 2916

Request article (free for British Glass members)

Size Scaling Of Tensile Failure Stress In A Float Soda-Lime-Silicate Glass
Int J Appl Glass Sci 1 2 2010 143-150
F 2916
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.