Size Effects On Silica Polymorphism

In this study, it was found that the polymorphism and sintering behaviour of silica can be affected by the size of starting particles. The formation of the stable tridymite phase, which is metastable unless a flux or mineralizer is present, is achieved with sintering of very fine silica particles of about 10nm without the presence of a flux or mineralizer. Cristobalite phase is obtained as an intermediate as the amorphous phase transforms into the stable tridymite phase.

Author
S Wu Et Al
Origin
Nat Tsing-Hua University, Taiwan
Journal Title
J Am Ceram Soc 85 10 2002 2590-2592
Sector
Special Glass
Class
S 2423

Request article (free for British Glass members)

Size Effects On Silica Polymorphism
J Am Ceram Soc 85 10 2002 2590-2592
S 2423