Situation Of The Waste-Heat Utilization In The German Glass Industry

A survey has been undertaken to establish to what extent waste-heat recovery units are used in the West German glass industry. Some 60% of factories in the survey had heat-recovery units, accounting for 75% of the total waste-heat available.