In Situ Observation Of The Dissolution Of Refractory Inclusions In Glass

The dissolution rate and bubble nucleation tendencies of zircon, Al203, Zr02, and AZS refractory in glass were measured utilizing hot stage microscopy in the temperature range from 1150 to 1400 deg C.