In Situ Measurement Of Glass Batch During Melting

A novel optical measuring method is described which was used for the density measurement of model samples of glass batch during the melting process. It used a sample volume of some 1000 mm3, which was sufficiently large to suppress single particle effects. Shape changes of batch samples during heating were taken into account by the optical method. Volumetric changes of soda-lime-silica glass batch were monitored between room temperature and 1100 deg C. Initially, a sintering stage was observed showing self similar reduction in the sample volume. Thereafter, the sample share approached the equilibrium surface of drops. This was accompanied by a large increase in volume, which was attributed to the formation of gas bubbles within the batch samples. A strong influence of heating rate and composition on this volume increase was observed.

Author
F Raether & M Krauss
Origin
Isc, Germany
Journal Title
Glass Sci Technol 77 3 2004 118-123
Sector
Special Glass
Class
S 2801

Request article (free for British Glass members)

In Situ Measurement Of Glass Batch During Melting
Glass Sci Technol 77 3 2004 118-123
S 2801
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
20 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.