In-Situ Investigations Of Sintering And Crystallization Of Lithium Aluminosilicate Glass-Ceramics

The sintering and crystallization behaviour of a Li20-Al203-Si02 glass powder containing Ti02, and Zr02 was investigated by the in-situ measuring methods of high-temperature dilatometry, high-temperature X-ray diffractometry and differential thermal analysis at heating rates between 0.5 and 20 K/min.