In Situ Degradation Of Ysz And Ysz + Al203 Electrolytes Of Sensors Used In Glass Melting Furnaces

This work reports on the degradation of pure YSZ and YSZ+10 wt% alumina composite electrolytes by exposure to the atmosphere of a heat recovery chamber of an industrial glass furnace at a temperature of around 1300 deg C. Microstructural observations and impedance spectroscopy measurements were used to evaluate the corrosion effects. YSZ samples directly placed in the sidewalls and intimately exposed to the dusts and atmosphere show strong corrosion effects after short periods. These samples present large amounts of a glassy phase in the intergrannular region, containing the same elements as the common batch with inclusion of volatile species from the fuel. At the same time, the average composition of YSZ grains remains almost unchanged.

Author
C M Rodrigues Et Al
Origin
Estg, Portugal
Journal Title
Glass Sci Tech 77 1 2004 17-24
Sector
Special Glass
Class
S 2694

Request article (free for British Glass members)

In Situ Degradation Of Ysz And Ysz + Al203 Electrolytes Of Sensors Used In Glass Melting Furnaces
Glass Sci Tech 77 1 2004 17-24
S 2694
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.