In Situ Chronoamperometric Analyses Of Individual Manganese Redox States In Glass-Forming Melts

Chronoamperometry was combined with square wave voltammetry for the in situ analyses of a series of manganese-containing glass melts at 1150 deg C. Glass melts containing 1wt% Mn were titrated with varying amounts of iron. Analyses monitored the changing manganese redox ion distribution caused by electron exchange reactions with the iron redox ions. This electrochemical technique shows promise for the in situ measurement of individual redox states in glass melts.

Author
M W Medlin Et Al
Origin
Virginia Military Institute, Lexington, Va
Journal Title
Ceramic Trans 82 1998 37-42
Sector
Special Glass
Class
S 1602b

Request article (free for British Glass members)

In Situ Chronoamperometric Analyses Of Individual Manganese Redox States In Glass-Forming Melts
Ceramic Trans 82 1998 37-42
S 1602b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.