In-Situ And 02 Laser Sensor For Burner Control In Glass Furnaces

A newly-developed laser sensor system for measuring CO and O2 in the burner ports of industrial glass furnaces is presented. Practical test results of the use of this sensor for monitoring the combustion process and for controlling the burners are given, for both an end-port fired regenerative furnace and an oxy-gas fired furnace. The use of the sensor for reducing NOx emissions and improving the energy efficiency of glass furnaces is demonstrated.

Author
A J Faber Et Al
Origin
Celsian, Netherlands
Journal Title
74Th Conf On Glass Problems 35 1 2014 103-108
Sector
General
Class
G 4419

Request article (free for British Glass members)

In-Situ And 02 Laser Sensor For Burner Control In Glass Furnaces
74Th Conf On Glass Problems 35 1 2014 103-108
G 4419
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.