Sisecam Invests In Its Highest Capacity Glass Packaging Furnace

Making significant contribution to the Turkish economy and employment, Sisecam Group will increase its annual glass packaging production capacity in Turkey to 1.2m/tons, together with the launch of a new furnace with an annual production capacity of 150,000/tons to be equipped with the latest Industry 4.0 technologies.