Sisecam Introduce New Single End Roving

Sisecam has introduced a new single end roving - WR5 - to the composites market. WR5 single end roving is made of E-glass fibers and is designed especially for weaving processes. Sisecam claims that the product has good unwinding, high process performance, no fuzz, lower tex count, fast and complete wet out and high mechanical properties. The silane based sizing is compatible with polyester, vinylester and epoxy resins. WR5 is being requested by weavers in multiaxial and woven reinforcement products and it is recommendable for marine, building and industrial applications.

Author
Un-named
Origin
Unknown
Journal Title
E-News Bulletin 9 May 2006
Sector
Glass Fibre
Class
GF 507

Request article (free for British Glass members)

Sisecam Introduce New Single End Roving
E-News Bulletin 9 May 2006
GF 507
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.