Sintering Kinetics Of Aluminium Oxide Ceramics With An Additive Of Eutectic Composition

Specifics of sintering of ceramics based on aluminium oxide with a eutectic additive are studied. It is shown that the sintering process proceeds in two stages: before liquid-phase formation in the system the main mechanism controlling sintering is rearrangement of the particles of the high-melting phase; after the liquid-phase formation in the system the main kinetic process is dissolution-precipitation. The main parameters controlling the kinetic process are the size of particles of the high-melting phase and the physicochemical characteristics of the eutectic melt.

Author
E S Lukin & N A Makarov
Origin
Mendeleev Russian Chemical Engineering University Moscow
Journal Title
Glass And Ceramics 57 1-2 2000 23 - 26
Sector
Special Glass
Class
S 3150

Request article (free for British Glass members)

Sintering Kinetics Of Aluminium Oxide Ceramics With An Additive Of Eutectic Composition
Glass And Ceramics 57 1-2 2000 23 - 26
S 3150
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.