Sintering Behavior Of Glass-Ceramic Frits

Combining DTA and HEMA data may provide as simple and quick method for describing the sintering/crystallisation process for different glass compositions.

Author
C Siligardi Et Al
Origin
University Of Modena, Italy
Journal Title
Am Cram Soc Bull 79 9 2000 88-92
Sector
Glass Ceramics
Class
GC 393

Request article (free for British Glass members)

Sintering Behavior Of Glass-Ceramic Frits
Am Cram Soc Bull 79 9 2000 88-92
GC 393