Sintering Analysis Of Undoped And Cobalt Oxide Doped Ceria Solid Solutions

Pure and CoO1-x-doped Ce0.8Gd0.2O1.9 (CGO) have been analysed with constant heating rate dilatometry. Doping changes the grain boundary structure of CGO resulting in enhanced mass transport and in increased densification rates. Significant changes in activation energies have been detected. While pure CGO exhibits a significant amount of surface diffusion, cobalt oxide doping enhances grain boundary diffusion. It is suggested that the sintering of CoO1-1-doped CGO occurs by rearrangement and grain boundary diffusion whereas grain boundary and volume diffusion govern the densification of pure CGO.

Author
E Jud Et Al
Origin
Inst Nonmetallic Materials, Zurich, Switzerland
Journal Title
Jacs 88 11 2005 3013-3019
Sector
Special Glass
Class
S 3022

Request article (free for British Glass members)

Sintering Analysis Of Undoped And Cobalt Oxide Doped Ceria Solid Solutions
Jacs 88 11 2005 3013-3019
S 3022
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.