Sintered Ceramic Materials Produced From Hydromica Clays

Results of studying the process of sintering of two similar-type ceramic mixtures made of three varieties of low-melting illite-containing clays with additives of nepheline sienite and synthetic pseudowollastonite are described. The expediency of using several varieties of simular-type clays with different mineralogical and granulometric compositions to expand the sintering interval is shown.

Author
G P Sedmale & U Ya Sedmails
Origin
Institute Of Silicate Materials At Riga Technical University, Latvia
Journal Title
Glass And Ceramics 57 1-2 2000 26 - 29