Single And Multiphonon Assisted Hopping Conduction In Co0-Te02-V205 Glasses

Glasses having a broad range of compositions in the system 10CoO.(90-x)TeO2.xV205 are prepared and investigated. DC conductivity, density, and molar volume are studied. The conduction mechanism is found to be nonadiabatic in nature. The activation energy for conduction, W, is found to be less than that of TeO2-V2O5 glasses containing Sn, Pb, and Bi oxides. Mott's model for the small polaron hopping conduction between nearest neighbours gives unreasonable values for the decay parameter of the wave function of the electron in the low valence state. The increase in the conductivity with temperature is interpreted in terms of the Schnakenberg model for an optical multiphonon assisted hopping process at high temperatures and single optical phonon process at the lower ones.

Author
E Mansour
Origin
Industrial Education College, Egypt
Journal Title
Phys Chem Glasses 46 1 2005 21-26
Sector
Special Glass
Class
S 2948

Request article (free for British Glass members)

Single And Multiphonon Assisted Hopping Conduction In Co0-Te02-V205 Glasses
Phys Chem Glasses 46 1 2005 21-26
S 2948
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.