Nogrid GmbH, the specialist supplier of meshless computational fluid dynamics (CFD) software, has introduced Nogrid pointsGlow, a software solution that simulates the glass container forming process and computes the results in full 3D. According to its German developers, the product is easy to handle and generates solid solutions. It can be used for BB, PB and NNPB processes.