Simulation Of Bubble Removing Process In A Tv Furnace

Growth and dissolution of bubbles generated during the batch reaction into glassy state is a very complicated physico-chemical phenomenon. Assuming that bubbles are removed by two mechanisms, flotation or absorption, a simulator to evaluate the overall influence of (a) glass and batch composition, including refining agents, (b) geometrical tank design, and (c) furnace operating conditions. For verification, the simulated results were compared with actual data from Nippon's TV panel furnaces.

Author
S Kawachi
Origin
Nippon Electric Glass Co Ltd, Japan
Journal Title
Ceramic Trans 82 1998 245-249
Sector
Special Glass
Class
S 1613a

Request article (free for British Glass members)

Simulation Of Bubble Removing Process In A Tv Furnace
Ceramic Trans 82 1998 245-249
S 1613a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.