Simulating By A Monte Carlo Method The Protection By A Surface Layer In Glass Dissulution

The presented Monte Carlo method solves the mathematics of transition state theory and describes the glass dissolution process on a microscopic scale. In the model, the glass is considered as a random mixture of a slowly dissolving, solubility limited component and a fast dissolving component. As the model parameters are similar to those in the Grambow model, the parameters of both models can be compared with each other, as well as with experimental values. The Mote Carlo method is used to investigate recent experimental results according to which the protection provided by the gel should be the major factor determining the glass dissolution rate. Although these results contradict the Grambow model, they are consistent with the presented simulations: protection by the gel is indeed important in glass dissolution.

Author
M Aertsens
Origin
Sck.Cen, Belgium
Journal Title
Ceramics Silikaty 43 4 1999 175-180
Sector
Special Glass
Class
S 1952

Request article (free for British Glass members)

Simulating By A Monte Carlo Method The Protection By A Surface Layer In Glass Dissulution
Ceramics Silikaty 43 4 1999 175-180
S 1952
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.