A Simple Direct Casting Route To Ceramic Foams

A simple direct foaming and casting process using ovalbumin-based aqueous slurries for fabricating ceramic and metal foams is demonstrated.

Author
S Dhara & P Bhargava
Origin
Indian Institute Technology, Kharagpur
Journal Title
J Am Ceram Soc 86 10 2003 1645-1650
Sector
Glass Ceramics
Class
GC 570