Silica Sand: Going Against The Grain

Interest in silica sand is booming, largely thanks to its use as a proppant in oilfield drilling, yet the mineral is used across diverse markets such as fillers and foundries. This article discusses different processing techniques and industry requirements.

Author
Un-named
Origin
Unknown
Journal Title
Ind Minerals June 2012 64-67
Sector
News Items
Class
N 2939