Significant Improvement Of Efficiency By Automatic Gob Control

For nearly two decades, Gedevelop AB has been a leading specialist in monitoring and control of hot glass flow in the glass fibre industry and has shown the way to enhance gob measurement and control in the glass container industry. The control of gob shape, weight and temperature has become essential for today's glass container operations and can have significant influence in helping to reduce production costs. This article presents the latest developments in the Gob Image Analyser concept.

Author
G T Laak
Origin
Gedevelop Ab Sweden
Journal Title
Int Glass Journal 124 2003 31-32
Sector
Container glass
Class
C 2054

Request article (free for British Glass members)

Significant Improvement Of Efficiency By Automatic Gob Control
Int Glass Journal 124 2003 31-32
C 2054
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.