Shield Regulator Protects Against Energy Loss

This article describes a Variable Shield Regulator, its application in the glass furnace process, and the energy savings it can obtain.

Author
A Castoldi
Origin
Stem Trafo, Italy
Journal Title
Glass International October 2012 30-31
Sector
General
Class
G 4050

Request article (free for British Glass members)

Shield Regulator Protects Against Energy Loss
Glass International October 2012 30-31
G 4050