Shear Spray Technology

Graphoidal Developments Ltd (Sheffield), received an order worth GBP 120,000 for 12 of its Single Feeder Shear Spray Systems from United Glass (Alloa). the installation and commissioning of the units was scheduled to be completed early in 2002. Graphoidal's systems which, says the company, are capable of accurately dosing at ratios of up to 1500:1 and use new technology shear oils, will be installed on each of the production lines at UG's glass plant.