Sgg Says Its U-Value Ko'S Competition

With its new SGG Climaplus Ultra double glazing, Saint-Gobain Glass says it has achieved a world first by obtaining the lowest heat loss coefficient (U-value) ever attained under normal manufacturing conditions.