Separation And Determination Of Lead And Barium Oxides In Glass Analysis.

Two methods of determining lead and barium in glasses are reviewed and investigated for use as controls in the works. These are:- separation and determination as sulphate using the different stabilities of their EDTA complexes in weakly acid solutions; separation as electro negative chloride complexes in an adsorption column with strongly alkaline ion exchanged. It is shown that only the ion exchange method is generally suitable in glass analysis. However, the first method is simpler and can be recommended for routine factory control of some types of glass.

Author
M Miscicka
Origin
Unknown
Journal Title
Glastechnische Berichte 44 11 1971 459-461
Sector
Primary Papers
Class
PP 1314

Request article (free for British Glass members)

Separation And Determination Of Lead And Barium Oxides In Glass Analysis.
Glastechnische Berichte 44 11 1971 459-461
PP 1314
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.