Sensor System Advances Gob Weight Control

Whilst developments in forming technology have advanced rapidly in recent years, improvements in forehearth technology have been slower. The feeder mechanism affects gob weight stability and so to solve this problem, a sensing system has been developed that can achieve significant advances in the control of the forming process.

Author
J Mcminn
Origin
Parkinson Spencer Refractories, Uk
Journal Title
Glass 76 6 1999 179-180
Sector
Container glass
Class
C 1357

Request article (free for British Glass members)