Sensor For Oxygen Partial Pressure Of Tin In Glass Float Bath

Measurement of the oxygen activity of tin used in the float glass forming process is crucial in determining the source of glass surface degradation. High oxygen content of the tin can result in tin surface bloom, glass staining and solar-control coating quality problems, as well as tin pick-up and cassiterite defects. If the operator knows the oxygen concentration of the tin, he can determine the optimum hydrogen concentration needed in various portions of the float bath.

Author
R F Conti Et Al
Origin
Heraeus Electro-Nite
Journal Title
The Glass Researcher 8 2 1999 13-15
Sector
Flat glass
Class
F 955

Request article (free for British Glass members)

Sensor For Oxygen Partial Pressure Of Tin In Glass Float Bath
The Glass Researcher 8 2 1999 13-15
F 955
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.