Semiconductor Passivation And Insulation Properties For Hydroxyl- And Fluoride-Free Zno-Sio2-B2O3-Al2O3 Glasses Stabilised By Increased P2O5

Fluoride- and OH-free phosphate-stabilised zinc boroaluminosilicate glasses for semiconductor passivation or insulation have been investigated with regard to compositional dependence of thermal expansion, viscosity and capacitor properties.

Author
K Kobayashi
Origin
Toshiba Vlsi Research Center
Journal Title
J Am Ceram Soc 1990 73 11 3500-3502
Sector
Special Glass
Class
S 459

Request article (free for British Glass members)

Semiconductor Passivation And Insulation Properties For Hydroxyl- And Fluoride-Free Zno-Sio2-B2O3-Al2O3 Glasses Stabilised By Increased P2O5
J Am Ceram Soc 1990 73 11 3500-3502