Self-Repair Of Glass And Polymers

Service life of glass composites is determined by fracture and corrosion. Delaminations and cracking are the major cause of structural failure. Development of fractures and catastrophic failure can occur on macroscopic and microscopic levels at one time, or in sequence. Safety glass as a composite is composed of two materials: the glass and the reinforcing fibres. One of the main common failures occurs at the interface between the matrix and the fibres. To prevent interlaminar failure and fatigue, good bonding between the matrix and the fibres is needed. Internal damage is also common in glass, especially corrosion damage. Repair of damage is important so that failures do not progress to the ultimate catastrophic failure of breakage. But corrosion damage is hard to detect unless it has developed to macroscopic scale flaws.

Author
C Dry
Origin
University Of Illinois, Usa
Journal Title
Cesp 64 Conf Glass Problems 25 1 2004 281-290
Sector
Flat glass
Class
F 1525

Request article (free for British Glass members)

Self-Repair Of Glass And Polymers
Cesp 64 Conf Glass Problems 25 1 2004 281-290
F 1525
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.