Self-Healing Glass Coating For High Temperature Applications (Abstract Only)

Glass-ceramics are a technological solution to achieve efficient materials to operate at high temperatures, such as for enamel protective coatings applications. To overcome cracking of the glass when subjected to thermal cycles self-healing is shown to be a promising solution. The self-healing property is defined as the capacity of a material to recover its mechanical integrity and initial properties after destructive actions of external environment or under internal stresses> Coillot et al, (Adv Funct Mat 2010) have shown that self-healing processing can be obtained in two different ways: Autonomous or Non-autonomous. Based on non-autonomous processing, an innovative approach is to develop self-healing glassy thin films for protective coating applications such as in the field of aerospace. This study is based on the heterostructure deposition of glass-ceramics and active particle layers by Pulsed Laser Deposition (PLD). The properties of the deposited films depend on many parameters during growth such as: number of pulse, frequency, energy density, atmosphere, temperature of the substrate, target-substrate distance, etc., We have shown that highly homogeneous layers of about 100-200nm are obtained under high vacuum, at room temperature, using a pulse energy of 225mJ, with a target-substrate distance varying from 3.5-5.5cm. The characterization of the multi-layer films has been studied using different techniques: Film thickness by ellipsometry; ToF-SIMS, AFM, Castaing microprobe; (ii) Homogeneity by Castaing microprobe, XPS; and (iii) structural characterization by ATR-FTIR spectroscopy. The efficiency of the self-healing effect is demonstrated by an in-situ experiment performed into an environmental scanning electron microscope (HT-ESEM).

Author
S Castanie Et Al
Origin
University Lille Nord De France
Journal Title
Icg Prague 2013 Abstract 058, 52
Sector
Glass Ceramics
Class
GC 835

Request article (free for British Glass members)

Self-Healing Glass Coating For High Temperature Applications (Abstract Only)
Icg Prague 2013 Abstract 058, 52
GC 835
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.