Segregation At Microscopic Flaw Peaks In Glass (In German)

The enrichment especially of alkaline ions on stress singularities (for instance microscopic flaw peaks) in glasses described analytically. A relation between the level of stress singularity and the number of atoms in the immediate neighbourhood is given.

Author
B. Rauschenbach And W. Hinz
Origin
Unknown
Journal Title
Silikattechnik 1979 30 (11) 329-331
Sector
Primary Papers
Class
PP 348