Seeing Clearly - Silica Processing Systems

As a low priced commodity, it is often less expensive to process a low grade ore body near the market place than to transport sand over long distances. As a result, silica sand process design is highly important to maximise returns on what can be a relatively low quality deposit. In this article the author review the different methods of processing silica sand alongside an illustration of how the discrete methods can be combined to produce a workable flowsheet.

Author
Un-named
Origin
Unknown
Journal Title
Industrial Minerals Feb/06 66-67, 69, 71
Sector
General
Class
G 3106

Request article (free for British Glass members)