Secondary Ion Mass Spectrometer Analysis Of Potash-Lime-Silica Glasses Leached In Hydrochloric And Sulfuric Acids

Results of tests on a glass of a composition resembling that of medieval stained glass showed that the kinetics of the acid leaching process are definitely influenced by the type and concentration of acid used.