Screenprinting On Glass With The New Sefar Pet 1500 Mesh

Screenprinting is the most universal technique for glass decoration. Various ink types, including opaque and transparent, can be used as well as conductive, insulating and adhesive pastes. In this paper the author looks at the factors considered for printing on glass, and describes what Sefar can offer for a variety of applications.

Author
R Drach
Origin
Sefar Ag, Switzerland
Journal Title
Glass Int Nov/Dec 2004 29-30