Screen Printing Inks For Glass

Today, many different glass objects are printed or decorated either directly or indirectly using the screen printing method. Every object to be printed will place different requirements on the chemical and mechanical resistance of the ink system used. Typical requirements include resistance to wear, dishwasher washing, weather, acids and so on.

Author
Un-named
Origin
Unknown
Journal Title
Int Glass Review 3/2000 145, 146
Sector
Enamels
Class
E 56

Request article (free for British Glass members)

Screen Printing Inks For Glass
Int Glass Review 3/2000 145, 146
E 56